Reference No.
Description
Expansion Coefficient (*10-7)
Firing Temperature (°C)
EGC-125
cast iron black enamel
334.2
760-780
EGC-126
332.4
EGC-622
thick cast iron black enamel
314.4
750-780
EGC-623
thick cast-iron black enamel
271.4
780-800
EGC-625
cast-iron black enamel
244.0
ECF-308
cast-iron transparent enamel
332.1
1271
274.0
1308
1309
335.5
740-760
2700
cast-iron opaque enamel
289.0
2707
acid resistant cast iron black enamel
2708
cast-iron white cover coat
2709
acid resistant cast-iron white cover coat
Note: enameling on surface of cast iron, as called Wet-way Coating enamel first, cleaning the surface of earthen bowl after anneal .
1 Milling additon ratio for cast-iron black enamel:
water
note: adding 10-20% quartz powder in acid resistant black enamel
0.5-1.0g/150mesh.100 ml
aluminium oxide
note: sub-opaque enamel consist of cast iron opaque enamel,with same milling addition ratio.
1-1.5g/150.100ml